Real-World Installations for Proven Durability
The following field installations have been completed to date:
Cell# |
Test Material |
Recap Presentation File |
|---|---|---|
| 1 | 75PC II/V + 25FA → 75% Portland Cement + 25% Fly Ash | (Coming soon) |
| 3 | 80PC II/V + 20FA → 80% Portland Cement + 20% Purebase (metakaolin-based SCM) | |
| 2 | 30BCSA + 70LC3 → 30% Belitic Calcium Sulfoaluminate Cement + 70% Limestone Calcined Clay Cement | (Coming soon) |
| 4 | 30BCSA + 70PLC → 30% Belitic Calcium Sulfoaluminate Cement + 70% Portland Limestone Calcined Cement | |
| 6 | 100LC3 → 100% Limestone Calcined Clay Cement | |
| 5 | 40PC + 10ReAct + 50GFBS → 40% Portland Cement + 10% Fortera ReAct® (reactive CaCO₃ SCM) + 50% Ground Granulated Blast Furnace Slag | Download recap slides |
| 7 | 100HPT → 100% High-Performance Ternary Blend (IT(L10)(P10)HS) | |
| 9 | 80PC II/V + 20KMI → 80% Type II/V Portland Cement + 20% KMI Zeolite (natural pozzolan) | |